to be honest the cold bluing kits are best avoided, I have tried several the caseys superblue being the least worst!
when you apply them they look okish, but they wear off very quickly, the only real option is to have the metal hot blued by a gunsmith, unfortunatly this costs, I have recently given up trying to source the equipment to hot blue , the costs of setting up are prohibitive, instead I have bought electro plating equipment and will try nickel plating my HW77 I am building for FT comps!